Hi Alex & other Technetters,
We manufacture MCB's at our facility and do a Direct plate ATOtech process
following a tetraetch. The process seems to work just fine.
Regards,
Les Connally
> From: Alex Stennett <[log in to unmask]>, on 7/14/98 12:19 PM:
> Has anyone considered the possibility of electroplating materials by
> applying a layer of conducting matereial first ...... I know it is a
> strange idea but I thought it might work and wondered if anyone was
> interested ................. ie I want to be in on the patent if it
> works!!!!!!!
>
> The process might cut out several stages in through hole plating too
> but it does mean changing the chemistry a little ............
>
> [log in to unmask]
> Alex Stennett
> Research Associate
> Loughborough University
> Dept. of Manufacturing Engineering
> Leics
> LE11 3TU
> Tel:- +44 (0)1509 228251
> Fax:- +44 (0)1509 267725
> -----------------------------------------------------------
> Add yourself to my Web address book at
> http://armadillo.lboro.ac.uk:591
> Enter the address_book.FP3 using guest as a password
> or just visit my homepage ........
> http://armadillo.lboro.ac.uk
> Or take in some small ads .....
> http://www.studentmart.com/
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################