I agree with Jim in that the argument that "you can't see it at 4X" is
pretty weak when in fact someone already found it (presumably at a lower
mag).
I think that you'ld find you'ld be better off dispositioning this in MRB
and being "up front" with you customer as opposed to attempting to
convince them you really can't see it at 4X. (I'm constatly suprised at
what can be seen at 4X).
Jim
================================================
James F Maguire
Associate Technical Fellow
Boeing
Information, Space & Defense Systems - Phantom Works
phone (253)657-9063
fax (253)657-8903
pager (206)982-3737
email [log in to unmask]
=================================================
> ----------
> From: [log in to unmask][SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;[log in to unmask]
> Sent: Thursday, June 25, 1998 6:42 AM
> To: [log in to unmask]
> Subject: [TN] Re2000A
>
> Hi Kenny:
> - You are correct in your understanding of the application of
> Mil-Std-2000A.
> Since you are obligated to produce hardware i/a/w 2000A it would be
> best to
> identify the solder balls as a "Defect." Then, take the defect into.
> to an
> MRB, and (with your customer present) conclude in the MRB that the
> sentence in
> par. 4.4 which says "Table 1 defects shall not be dispositioned "use
> as is.""
> should not be applied to this defect. If the conditions are as you
> described,
> there would seem to be no logical reason to proceed with a repair.
> Once upon
> a time (back when Mil-Std Category A's roamed the world) there was a
> person to
> whom you could appeal such things based on technical merit,
> unfortunately that
> condition no longer exists and you need to work something out with
> your
> customer.
> Hope the above helps some, if not - contact me direct and we can
> discuss
> alternatives.
> Jim Moffitt, Moffitt Enterprises
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|