Matt, non wetting of a pad or land after HASL is very possible. My
guess is the large areas had exposed CU on reciept. In the areas around
the annular ring, may be a little Solder mask "bleed-out" or other
Solder mask related issue. The chances of somethin chompin it off
during component attachment is slim.
Hope this helps,