We use metal blades. Fiducials are not cut all the way through, just part
way. Then they fill them with a dark colored epoxy. I did have change the
video recognition too light to dark for the DEK 265 system to recognize
them, but that was the only change.
Thanks,
Kathy Palumbo
> ----------
> From: McMonagle, Michael R.[SMTP:[log in to unmask]]
> Sent: Monday, July 06, 1998 10:23 AM
> To: [log in to unmask]
> Subject: Re: [TN] Polyimide See Thru Stencils for Printing Solder
> Paste
>
> What type of blades are you using? How do they mark stencil fiducials,
> full cut through?
>
> Mike McMonagle
> K*Tec Electronics
>
> > -----Original Message-----
> > From: Kathy Palumbo [SMTP:[log in to unmask]]
> > Sent: Monday, July 06, 1998 11:26 AM
> > To: [log in to unmask]
> > Subject: Re: [TN] Polyimide See Thru Stencils for Printing Solder
> > Paste
> >
> > Johannes,
> >
> > I have tried this type of stencil. It was made by a company in Canada
> > called KJ Marketing. It worked extremely well. The material is laser
> > cut,
> > and as a result of the heat from the Laser the walls of the apertures
> > are
> > perfectly smooth. The release of paste was outstanding. It performed
> > as
> > well or better than a pure nickel stencil.
> >
> > Alignment was made easy due to the ability to see through the stencil.
> >
> > The material can be melted down and used again, and it does not
> > stretch as
> > much.
> >
> > You should try it out yourself and see what you think.
> >
> > Thanks,
> > Kathy Palumbo
> > > ----------
> > > From: Johannes Sivula[SMTP:[log in to unmask]]
> > > Sent: Tuesday, June 30, 1998 4:18 AM
> > > To: [log in to unmask]
> > > Subject: [TN] Polyimide See Thru Stencils for Printing Solder
> > Paste
> > >
> > > Polyimide See Thru Stencils for Printing Solder Paste
> > >
> > > Following mail was posted by Russ M on June 23, 1998 at 11:27:37:
> > to
> > > http://www.smtnet.com/smt_forum/smt_mail.html
> > >
> > > Has anyone seen/used these yet? They seem to have lower
> > > coefficient of friction
> > > for release of paste and less wear and tear as well as
> > > conforming to the board better
> > > (plastic has better memory than stainless). Also there is
> > no
> > > mesh
> > > so a larger
> > > image can be put in a smaller stencil size. But, the best
> > is
> > > that
> > > you can see through
> > > the stencil for manual and semi-automatic printer
> > alignment and
> > > reduce set up and changeover times.
> > > Anyone familiar with these?
> > > How long do they last?
> > >
> > ----------------------------------------------------------------------
> > ----
> > > -
> > > ----------------------------------------------------------
> > > Any comments ?
> > > brs, Johannes
> > >
> > >
> > >
> > > This type os stencil is available from:
> > > KJ Marketing Services
> > > 115-30th St.
> > > Toronto, Ontario, M8W 3C1
> > > Phone: (416) 252-1061
> > > Fax: (416) 253-1687
> > > email: [log in to unmask]
> > > Web Site: www.kjmarketing.com
> > > Regards John Parsons Circuit Graphics Ltd. [log in to unmask]
> > >
> > > ################################################################
> > > TechNet E-Mail Forum provided as a free service by IPC using
> > LISTSERV 1.8c
> > > ################################################################
> > > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > > following text in the body:
> > > To subscribe: SUBSCRIBE TechNet <your full name>
> > > To unsubscribe: SIGNOFF TechNet
> > > ################################################################
> > > Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> > > section for additional information.
> > > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> > > 847-509-9700 ext.312
> > > ################################################################
> > >
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> > 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> > section for additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> > 847-509-9700 ext.312
> > ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|