Charlie-
I was under the impression that you would atach the fax (thermal) to
the top of an unpopulated board. This would show you if and where flux
was penetrating to the topside. Without sufficient flux in the
through-holes, it is difficult to get good topside fillets, etc.
Ryan Jennens