Earl Moon wrote:
> It has recently, and disruptively, been brought to my past ignorant
> attention the problem associated with electroless nickel deposition
> under electroless gold deposited SMT solder termination areas. I have
> been informed, by a major BGA supplier, the deposition process relies
> on
> phosphorous as a component in the plating solution. Further, I have
> been
> told this is detrimental to solder joint formation.
>
> It is said, and has been proven by the BGA supplier, that phosphorous
> causes solder joint problems by forming an internetallic that, over
> time, causes embrittlement. Therefore, solder joints fail.
>
> Has anyone in industry addressed this issue from a PCB fabrication
> standpoint? If so - how, and what is being done? Can we specify
> electroplated nickel in approximately 100 millionths thickness as for
> electroless types? If so, will this overcome the intermetallic,
> embrittlement, and solder joint problem?
>
> Thanks, Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
Hi, TechNetters!
Earl Moon refers to BGA joints . What about all the SMD joints?
Did Pandora again open her box?
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|