Subject: Re: [TN] Re[2]: [TN] Conformal coating
Eden,
By the sounds of your question, I think you need to take a look at the
"real" problem here before jumping to any conclusions. Does your PCB
even need conformal coating from an operating environment standpoint?
Don't use it to "band-aid" a real problem, which in this case would
make it worse. It sounds like you need dryer PCB's from your vendor
(look at their process; are they using treated H2O in their washes?).
I would not get into doing conformal coating if you really don't need
it!
Mark Pozorski
Sr. Mfg. Eng.
ADC Telecommunications
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|