First thing to do is run a profile. I would test cross belt temperature
uniformity and rise rates. MOST IMPORTANT - get a copy of the recommended
reflow profile for the solder paste manufacturer. Ensure you are meeting all
specs like rise rate, soak time, time above reflow, etc.
Brian Stumm
a reflow manufacturer
>Hi,
>
> Need some advice on how to eliminate or reduce the solder on finger
>that
>we are having right now. So far what we understand is that 90% of the
>problem is
>due to the reflow process where solder traps in vias causing explosion when
>subjected to high temp during reflow. Not sure whether this is the right
>assumption but from what we have seen on the reject there are solder balls
>all
>over the 'exploded' vias. The signature of solder on finger defects is
>10-40
>mils of 'dot' which could be caused by solder balls. SO this is my
>questions:
>
>1. Is it possible that the vias can 'explode' during reflow?
>
>2. Does the ramp from room temp to soaking time(145-160 deg C) and from
>soaking
>time (160-183 deg C) play an important role in determining the amount of
>'explosion'. So far our data shows that it does.
>
>3. Is there any other possible causes of solder explosion...Solder paste?
>
>
>Thank you and really appreciate the help.
>
>Masdi Muhammad,
>Process Engineer.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
ETS, LLC - West ETS, Inc. - East
3939 N. Freya St. PO Box 47887
Spokane, WA 99207 Plymouth, MN 55447
509-483-0900 (voice) 612-553-0051 (voice)
509-483-0331 (fax) 612-553-0246 (fax)
[log in to unmask] [log in to unmask]
Benefit from a direct relationship with the manufacturer!
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|