I believe there are some films made by Agfa called CPN and CPFab that
might work for date codes.

> ----------
> From:         Lisa Parker[SMTP:[log in to unmask]]
> Sent:         Friday, July 17, 1998 9:03 AM
> To:   [log in to unmask]
> Subject:      [TN] Diazo adhesive transfer film
>
> We used to buy a diazo adhesive transfer film from Glenbrook
> Technologies (P/N IP2-LIT-MAT  size 8.5x11, 2 mil clear, sepia
> standard
> speed, Imtac).  This is no longer available from Glenbrook, Rexam,
> GMP,
> Morton.  Apparently no one manufactures this film any more.
>
> If you have some of this film (brand or size is not important) I would
> like to buy some.  Do you have any suggestions as to what to use
> instead
> of this.  (We use it for date codes on artwork.)
>
> Lisa Parker, Purchasing Agent
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2