I resently had a customer increase their peel strength from 1 pound to 15
pounds by creative use of our AT2000 product. The process is to expose the
nickle foil to a 2% concentration of out AT2000 in water. I can't tell you
why it worked but it did. If you think this may help you feel free to e-mail
me back.
Scott Griggs
Senior Applications Engineer
RBP Chemical Corp.
[log in to unmask]
################################################################