It is 1453C. For future reference on such, try my favorite sites for Web
based Periodic Tables:
http://bvsd.co.edu/~stanglt/per.htmlhttp://beta-tech.mit.edu/Chemicool/
MikeMcM
> -----Original Message-----
> From: Ruben Irizarry [SMTP:[log in to unmask]]
> Sent: Thursday, July 16, 1998 10:31 AM
> To: [log in to unmask]
> Subject: [TN] Nickel Melting Point
>
> I am in a rush and need thwe melting point of pure Ni. Will someone
> help
> me?
> Thanks in advance
> Ruben
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################