Chris,
Does 'organometallic tin' mean a co-deposited polymer?
Steve
I am aware of the Dexter Dexcoat FST process. This is an organometallic tin
that places a barrier layer on the copper surface that greatly retards the
copper tin migration to a point that shelf life well in excess of one year
is
easily achievable. This process produces a lead free planar surface that has
better solderability than Ni/AU. Some OEM's have claimed that this process
is
the only alternative finish that they can run on the same assembly line with
HASL product and no changes need to be made. The key here is that the
process
in not an ordinary immersion tin which would have a very limited shelf life.
Regards,
Chris McGary
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|