TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Hütter Simon <[log in to unmask]>
Date:
Mon, 6 Jul 1998 07:59:24 +0100
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Hütter Simon <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Hello Techneters.

I have heard that the phosphorous content of electroless Ni
should be more than 10% to avoid microcracks in the Ni
under the Au. Also it should be better for wire bonding.

But on the other hand it must be less then 10% for a good solderability
(discussed here before).

Our electroless Ni/Au has a P content of 8-10%. And the supplier says
that this is perfect for soldering and wire-bonding.

Can anyone help me out of this?

Thanks
Simon

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2