Hello Technet,
What are users of Alpha Metals flux 615/16 or 615/25 using as
thinner ?
The official Alpha 443 thinner is a lot more expensive than a good
grade isopropylalcohol, and upto now Alpha didn't gave me a real good
reason for not using isopropylalcohol. I recently switched to the
Alpha 443 thinner because of explicit recommendations from Alpha,as
soons as they're running in delivery-problems the supplier tells
us that this is due to the fact that we are their only customer for
this thinner and they have to import it especially for us ! Sounds
like other companies are using isopropylalcohol, but I'd like to hear
this from actual users of the flux.
Daan Terstegge
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|