TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 30 Jul 1998 21:58:21 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Joseph E. J. Duclos Jr." <[log in to unmask]>
Subject:
From:
"Joseph E. J. Duclos Jr." <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (51 lines)
I would agree with your formula, however, when I met Mark Simmons at IPC
EXPO 1997 he pointed out that tip wear was indeed a measurable factor.
Basically, I would do(and did) the following:

1) Find out the 'worst case' tip wear, i.e.: how short the flat or rounded
cutter of the blade is from a perfect point before re-sharpening [in my
application .005"]
2) Determine your manufacturing tolerance of artwork (registration,
dimensional stability etc..) [in my application .006"]
3) Now the math parts, use the .021 and add the .005 to it, then apply this
to your formula.
A) In addition, in my case I would account for the web not being centered by
adding and additional .001-.002.
4) The answer to this particular instance, for me, would have been .022".

JOE SENDZ......

(Joe Duclos - TYCO Printed Circuit Group, Stafford Division)


If you would like to contact me on or off line for more info
[log in to unmask]


-----Original Message-----
From:   TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent:   Thursday, July 30, 1998 12:42 PM
To:     [log in to unmask]
Subject:        [TN] Scoring

     I am looking for input as to what others use as a rule for cutting
     back copper on artworks

        <<<SNIP>>>

                                 Thanks

                                 Ernie Smith    [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2