TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Thu, 30 Jul 1998 19:06:57 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (61 lines)
In a message dated 98-07-30 16:45:10 EDT, you write:

<< Hi Jeff

 Always thought that closeness of SMD components to scorelines was a much
 neglected subject. In another life I had some bad bad experiences with
 this....

 Wolfgang / Viasystems Canada

 >      BTW Mark,
 >      I notice that there are no references to guidelines for
 >      closeness of SMD components to V-score edge..any feedback from the
 >      industry or feelings for this subject you would like to share
(please,please).
 >      How about anyone else out there?
 >      Regards & Thanx!
 >
 >      Jeff Hempton
 >      United Technologies Electronic Controls
 > >>

Hello Wolfgang, and Jeff!

If you want to talk to someone who has done a study on exactly that subject,
call a gentleman named Dennis Johnson at: (510) 262-8990, he's the owner of a
company named "Onanon", and what they do for a living is nothing but drilling,
scoring, and routing. Dennis was asked by 3COM to determine how close they
could put a capacitor to a score line and not worry about damage during
singulation, and that's exactly what he did.

Dennis and his company bailed me out one time when we got a consigned job that
had scored panels. Problem was, the fabs we recieved weren't scored deep
enough.
Even worse, that little tidbit of information wasn't discovered until after
the boards were built (says something about our customers incoming recieving
inspection don't it?). So this was just peachy, we got the boards built, but
couldn't get them out of the panel. Dennis was able to pull a rabbit out of
his hat, and go back and re-score them to the proper depth with the boards
loaded. Needless to say, I owed him a few lunches for that one.

He's also developed a chart that you can use to determine what a good depth
for scoring is. It's based on what the laminate thickness is, and how big the
individual PCB in the panel is, and it really works! I use it every time I
need to come up with a scoring spec, and it hasn't once let me down. I've used
it mostly with PCMCIA, and SIMM panels.

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2