Todd,
In our experience, the reason most people run between 235-250C is twofold: it produces less dross
and it gives the flux (especially No-Cleans) the best environment in which to be effective. In
many cases where a higher temperature is used, it was done to compensate for high levels of
oxidation or was implemented from a different process. Not knowing board thickness, component
quality, or density, it is likely that going to a lower temperature may produce a shinier fillet,
good wicking, and less dross in the pot.
Phil
Running at 261C will
Todd Ness wrote:
> Hi,
>
> I would like to know the differences between having our solder pot
> temp for 63/37 solder at 261 Degrees C instead of 250 Degrees C. Will
> we see less bridging and better top-side flow at the higher temp? Are
> there any pros and cons for the different temperatures?
>
> Thanks,
> Todd N
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|