TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Russell S Gregory <[log in to unmask]>
Date:
Mon, 27 Jul 1998 15:34:28 EDT
Content-transfer-encoding:
7bit
Content-type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (34 lines)
Dear Technetters,

There does not appear to be an industry standard acid resistance test for
determining the functional quality of a reduced black oxide layer. The acid
resistance test is a good method for determining the quality with respect to
pink ring resistance.

Several companies and indeed suppliers have different methods for testing this
functionality of the Reduced Oxide process.

So I thought it might be worthwhile firing these questions off around the
world :
What method is used at your shop to test the acid resistance of your Reduced
Black Oxide process - in terms of acid type - strength and application method
and when is it tested?

If you are using an alternative oxide or oxide replacement do you still carry
out an acid resistance test?

Russ Gregory
Atotech UK

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2