Start throwing money...
Externally, for a bulletproof design, you'll need Teflon, PVDF, titanium or
some FRP composite.
As previously mentioned, you're best off with an in-tank design, where CPVC
will work - providing there are NO glue joints (i.e., threaded or flanged
w/ Ti hardware). Polypropylene might work too, since that's what the
filter material is likely to be.
J.Felts
-----Original Message-----
From: Chris Rucinski [SMTP:[log in to unmask]]
Sent: Monday, July 20, 1998 11:07 AM
To: [log in to unmask]
Subject: [TN] Black Oxide Filtration
Could anyone help me find a pump and filter
house material and/or brand name that will
withstand black oxide chemistry. What are
other circuit board manufacturers using? I am
most interested if a board manufacturer has
been able to overcome this problem without
throwing lots of money at it.
Vendors please contact me direct.
Thanks in advance
Chris Rucinski
Process Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|