Mime-Version: |
1.0 |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Mon, 20 Jul 1998 09:08:40 +0800 |
Content-Type: |
text/plain; charset="us-ascii" |
X-To: |
|
Reply-To: |
|
Parts/Attachments: |
|
|
>Received: from jefry.ipc.org (jefry.ipc.org [208.150.51.11]) by
asiaonline.net (8.8.6/8.7.3) with ESMTP id FAA05164 for
<[log in to unmask]>; Mon, 20 Jul 1998 05:01:41 +0800 (HKT)
>Received: from jefry (208.150.51.11) by jefry.ipc.org (LSMTP for Windows
NT v1.1a) with SMTP id <[log in to unmask]>; 19 Jul 1998 15:44:25 -0500
>Received: from JEFRY.IPC.ORG by JEFRY.IPC.ORG (LISTSERV-TCP/IP release 1.8c)
> with spool id 832624 for [log in to unmask]; Sun, 19 Jul 1998
> 15:44:24 -0500
>Received: from simon.ipc.org by jefry.ipc.org (LSMTP for Windows NT v1.1a)
with
> SMTP id <[log in to unmask]>; 19 Jul 1998 15:44:24 -0500
>Received: from mail-out-0.tiac.net by simon.ipc.org via ESMTP
> (951211.SGI.8.6.12.PATCH1502/940406.SGI) for <[log in to unmask]> id
> PAA24878; Sun, 19 Jul 1998 15:50:15 -0700
Hi,
I got another one....
Glass Paper (AKA Composites - - - CEM-1, 22F)
BT resin
regards
Jens Behrens
http://www.felsweb.com/lam_faq.htm
>I am trying to construct a PCB supplier survey outlining all base
>materials available. Currently my list consists of:
>
>Phenolic (XXXPC< XXPC, XPC, FR2, FR1)
>Epoxy Paper (FR3)
>Epoxy Glass (glass woven fabric >FR4/G10 + glass felt >> CEM-3)
>Polyimide Composite
>Polyimide Glass
>Cyanate Ester
>Flex Materials
>Teflon = PTFE
>GETEK
>
>Have I left anything out? If so, please advise so that I can make the
>necessary additions. I would like to thank all that participate for
>their time.
>
>Best Regards
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|