> Jerry,
>
> We recently did some testing of "double sided reflow" related to
> reliability. In our testing we were wondering if reflowing a 2nd time
> with the part on the "bottom" of the PWB (so gravity pulls the part away
> from the PWB surface) would impact reliability (and also, if it would
> stay in place during reflow).
>
> Our results showed a) it stayed in place and b) no impact on reliability
> (we've passed >1600 cycles -55/125C thermal shock with 30 min. dwells at
> temp per side without any electrical intermittents.
>
> Jim
> ================================================
> James F Maguire
> Associate Technical Fellow
> Boeing
> Information, Space & Defense Systems - Phantom Works
> phone (253)657-9063
> fax (253)657-8903
> pager (206)982-3737
> email [log in to unmask]
> =================================================
>
> > ----------
> > From: Jerry Cupples[SMTP:[log in to unmask]]
> > Reply To: TechNet E-Mail Forum.;Jerry Cupples
> > Sent: Tuesday, June 23, 1998 3:15 PM
> > To: [log in to unmask]
> > Subject: [TN] ASSY: BGA sanity check
> >
> > Hello, TechNet....
> >
> > Soldering (inline convection furnace) BGA's on both sides of a board
> > is
> > beyond my own experience, but it seems to violate a principle (at
> > least an
> > imaginary one) related to the controlled collapse, or perhaps liquids
> > under
> > tension.
> >
> > For a board design using 3 commercial BGA packages (PBGA 256, eutectic
> > balls on 1.27 mm pitch), am I obstinately blocking the path of
> > progress by
> > requesting that this package style be confined to only one surface of
> > a new
> > board design?
> >
> > If you are doing this today and it is a piece of cake, go ahead and
> > brag;
> > but I would prefer to hear that caution is well advised, i.e. tales of
> > misery, shame and corporate disaster resulting from such mistakes. ;-)
> >
> >
> > cheers,
> >
> >
> >
> >
> > Jerry Cupples
> > Interphase Corporation
> > Dallas, TX USA
> > http://www.iphase.com
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> > 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> > additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> > 847-509-9700 ext.312
> > ################################################################
> >
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|