Specs from laminate manufacturers show a substantial difference in
coefficient of thermal expansion between X-axis and Y-axis for FR4, FR2,
CEM3, CEM1, etc. Is there any way I can tell from a finished PCB which is X
and which is Y? How can I specify in my PCB drawing such that a fab. house
always orientates my PCB in a particular axis? I consider this as a mean to
match with the CTE of certain components on that PCB.
Thanks!
K.K.Chin
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|