to acheive better throwing power i.e. surface to hole ratio in high aspect
ratio plating you can do one of the following:
Plate at lower current density for alonger time (less productive).
Use an additive system that has more suppression, it will suppress plating in
the higher current density (CD) areas, or the surface, and allow the lower CD
areas, in this case the middle of the hole, to catch up.
Use pulse reverse plating where the CD is redistributed ( Electrically) to
acheive the same goal as above.
I hope this helps.
George milad
Technical Marketing Manager
LeaRonal Inc.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|