TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Bogdan Gabi <[log in to unmask]>
Date:
Tue, 14 Jul 1998 16:48:33 +0200
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bogdan Gabi <[log in to unmask]>
Parts/Attachments:
text/plain (23 lines)
Don,
We have very limited experience with tin immersion boards.
The last board I checked in wave soldering was different from the first
supplier's by showing the white residues I called "wax like".
I also thought that there must be a connection with the no clean flux,
the HASL boards don't show this phenomenon either.
We were not able to achieve good results with any of the samples we got
till now.
I wish you success.
Gaby

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2