[log in to unmask] wrote:
> Steve,
>
> There is actually a trace amount of another metal codeposited with the
> tin.
> This is what also eliminates whiskering. There is an organic deposited
> on the
> surface which serves as a oxidation inhibitor for the final finish.
> This is
> then burned off at the wave.
>
> Regards,
> Chris McGary
> (800) 877-9871 ext209
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
Hello, TechNetters
We are also trying to evaluate immersion tin in our facility.
I am looking for some indications concerning solderability with no clean
fluxes, dwell time between soldering steps, storage and handling.
My first wave soldering test done with no clean flux in the same
conditions as with HASL boards was not very encouraging. Maybe that I
didn't know what special measures to take.
Some white stuff like wax showed up on pads and in on1/3 filled holes
....?!
Compatibility with our flux?
Soldering profile?
Bad luck?
Tin thickness with XRF: 0.4um. !!
I did not find any matter of fact answers concerning this process on the
net. Maybe it's too early?
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|