TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Wed, 8 Jul 1998 08:47:06 +0000
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Edwin Maximo <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
7BIT
From:
Edwin Maximo <[log in to unmask]>
Comments:
Authenticated sender is <emaximo@[192.1.1.215]>
Parts/Attachments:
text/plain (23 lines)
Hi!
Does anyone here have experience using a Black Epoxy in removing the
top marking of an IC. Can you site what is its advantages and
disadvantages when it is being use and also do you know where can I
purchase this epoxy and how much does its cost.
Any information given will be appreciated.

Thanks and regards,
Edwin Maximo
Electronic Assemblies Inc.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2