     I think you will find upon analysis (chromatography or FTIR) that
amine antistatic agent and diallyl phthalate plasticizer are the two
contaminats from pink poly.  I know the amine can cause solderability
problems.  Perhaps a mild etch could be used prior to soldering or a
more highly activated flux.

Pat Hogue
Materials and Processes
[log in to unmask]

> ----------
> From:         Mike Bailey[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Mike Bailey
> Sent:         Thursday, June 04, 1998 7:33 AM
> To:   [log in to unmask]
> Subject:      [TN] Anti-Static Bags
>
> Has anyone experienced problems with packaging bare PCB's in the pink
> anti-static bags?  We are seeing a "waxy"image transfer from the bag
> to
> the panel after what appears to be several months of storage in a
> controlled atmosphere.  It is aggravated by stacking individually
> packaged boards on top of each other and has occurred on several
> different surface finishes. The substance can also be found on the
> non-board side of the bag.  Does anyone know of  what the coating
> might
> be comprised?  Would you predict solderability issues etc?
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2