Hi,

  We recently went through an exhausting excersize with tantalums.   The
  vendor we used to assemble a small lot was not using pre-heat at the
  wave solder.  The tantalums were thermally overstressed.  When
  testing at ATE, we experienced some firecrackers.   After a back
  and forth with the component manufacturer I became convinced that
  these tantalums(can't speak for all)  were damaged from excessive
  heat.   Well we beat up our assembly vendor and also learned something
  new.

  Good luck

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2