Tom,
There are differences between plate and hot dip soldering. Hot dip provides a better coverage of
the base with less opportunity for oxide development because of the uniformity of the coating and
less porosity than plating. Additionally, it gives a better cosmetic finish that is shinier than
plated.
Of course, we are flux manufacturers and biased, but our feelings are also reflected by companies
that used to plate and have switched to soldering.
Phil
Tom Lambert wrote:
> Hi Folks : I just know many of you out there have knowledge re termination
> finish of chip parts to pass along. Specifically - is "hot solder dip" any
> better/worse than "solder plate" ?? Thanx.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|