Hi Bill - thanks for the followup - it puts my faith back in a few physics
principles! I'll file this one in my unique but possible defects file.
Dave
Bill Fabry <[log in to unmask]> on 06/23/98 04:45:28 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TN] Gold Coated Solder - a Followup
Techies:
Thanks for your response to the above-mentioned topic.
As it turned out, the root cause of the problem wasn't as difficult or
"off-the-wall" as I originally thought it to be. Steve Gregory hit the
nail on
the head.
Our assembly subcontractor splashed solder on the adjacent gold fingers
during
component replacement. They used in-house gold replating operation to
resurface
the fingers and were a bit overzealous in the plating, causing the MELF
terminals to be inadvartantly coated along with the fingers with the "new"
gold.
Bill Fabry
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################