TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"(Jim Hepburn)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 1 Jun 1998 13:13:57 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (71 lines)
Tim,
Try one of these. I have used them both in the past.

EMC Global Technologies
4059 Skyron Drive
Doylestown, Pa 18901
(215) 340-06450
The inside Sales Rep was K. Martin Wetzel

TK Machining
RT 202
Waterboro, Me 04087
(207) 247-3114
Bob DeWitt

Good Luck
Jim Hepburn
Objective Communications




"Stammely, Tim" <[log in to unmask]> on 06/01/98 11:18:24 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Stammely, Tim" <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Jim Hepburn/OCOM)
Subject:  [TN] Selective Soldering Pallets for Wave Soldering




Can anybody point me in the direction of a manufacturer(preferably on the
east coast) of selective soldering pallets for a mixed assembly board we
are
going to Wave Solder. Thanks in advance.

Tim Stammely
Process Engineer
MSI
Manassas, VA
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2