To Rudy Sedlak, Aric Parr and Dave Andersson, thank you for your short
lessons in what happens when you solder silver epoxy on a soldered
surface. We had a meeting and the words from you are in the one end of
the balance now, and went to the floor with a bang. So, we decided
immediately to a)rub the thin solder plating with Scotch Bright down to
the Nickel plating, and hence put adhesive on Nickel instead fo solder
b)try to fuse the solder plating first and then glue.
What a wonderful roadrunner answer, thanks again! I think we find our
way out by this.
Ingemar Hernefjord
Ericsson Microwave Systems
|
|
|