Keith, further to our discussion, I would like to confirm the action items:
The reason for failure is due to insufficient soldermask thickness over
conductors. During my last visit, plating thickness control was
discussed.
To improve the current situation please do the following:
1) Mesh size use a 38 T screen for boards that require NiAu.
2) Compare the results / process consistency by evaluating a partial
cure process.
Cure boards for 30 minutes at 150C, plate, and then cure for another 30
minutes.
With regard to plating process control, you may want to discuss this with
Barry, conductor heights in the range of 85 / +100 microns are difficult to
reliably encapsulate.
I have spoken to Tony Hunt, he will contact you shortly. In the meantime if
you would like to discuss further please give me a call.
Regards
Fred
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|