We have a FR-4 board (11" by 8" by 0.093") on which is mounted a large
sink beneath two power transistors. When the screws which secure the
transistors to the heat sink and to the board are torqued to 5
inch-pounds, significant measling beneath the heat sink (visible from
solder side) occurs when the board is flow soldered. When the torque is
reduced to 3 inch-pounds the measling disappears.
Does the above information suggest there is a problem here beyond a
simple process problem which is addressed by reducing the torque from 5
inch-pounds (which the drawing specifies) to 3 inch-pounds? (For the
record, I don't know if this should be called measling or crazing--both
the mechanical and thermal stress are required to produce the
phenomenon.
It seems odd that the relatively small amount of torque change could
have such a dramatic effect--if the material is within specification
limits and the flow solder process is close to optimal.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|