> I would like to hear if anybody have experience wtith a cleaning process of
> PCB-boards after plating with electroless copper. Does anybody brush the
> boards or use a chemical treatment etc.
>
> Regards
>
> Jacob Ransborg
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################Jacob,
Most electroless copper deposits are fairly rough in terms of topography
and generally provide an excellent surface for dry film adhesion.
Generally, no precleaning after electroless is required if you are going
directly to imaging.(assume hold times between electroless and
photoresist lamination is less tha eight hours)
Depending on deposit thickness, scrubbing is not recommended anyway.
Good luck.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|