Michael,

low cost PTFE/woven glass base materials are TLC-30 (DK 3.0), TLC-32 (DK 3.2), and RF-35 (DK 3.5) from
Taconic. All of them are used at the frequency range you described.

Please contact us off-line to discuss further.

Regards

Manfred Huschka
Taconic Advanced Dielectric Division Europe


--- On Tue, 16 Jun 1998 15:08:12 -0500  Michael Thiel <[log in to unmask]> wrote:
I would like to know the options available, as far as board
material/conductor and its
 characteristics, for an application involving frequencies ranging from
500mhz to 2ghz (with the upper
 limit (2ghz) being more of a concern). Intentions are to emphasize
microstrip matching at higher
 frequencies (2ghz) and lumped component matching at lower frequencies
(500mhz). Basically, what
 works the best and is cheap.

 Thank you for your cooperation.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################



---------------End of Original Message-----------------

--------------------------------------------------------
Name: Manfred Huschka
Taconic Advanced Dielectric Division, Lynn Industrial Park, Mullingar,
Co. Westmeath, Republic of Ireland
Office: PF 1275, D-51676 Wipperfuerth, Germany
        Tel.: +49 2267 888004
        Fax:  +49 2267 888005
E-mail: Manfred Huschka <[log in to unmask]>
Web: www.taconic-add.com
Date: 06/17/98
Time: 09:50:08

This message was sent by Z-Mail Pro - from NetManage
NetManage - delivers Standards Based IntraNet Solutions
--------------------------------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2