Sorry - I don't mean to advertise - but you can get this paper (or the
entire proceedings) from us. Reprints of SMTA papers are free for our
members.
-David
At 12:06 PM 6/16/98 -0500, you wrote:
>Hi Steve - take a look at the following paper:
>
>"Ball Grid Array, MicroBGA, Chip Scale Packaging, and 0.4mm Ultra Fine
>Pitch Implementation At US Robotics", author Ron Evans, et al, pages
>141-163, SMTA National Symposium "Emerging Technologies" Proceedings,
>October 1997"
>
>The paper contains some good information on ball grid array pad design and
>manufacturing interaction issues that may be relevant to your issues. Good
>Luck.
>
>Dave Hillman
>Rockwell Collins
>[log in to unmask]
>
>
>
>
>
>"Joy, Stephen C" <[log in to unmask]> on 06/16/98 11:33:00 AM
>
>Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
> to "Joy, Stephen C" <[log in to unmask]>
>
>To: [log in to unmask]
>cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
>Subject: [TN] Solder mask profile information
>
>
>
>
> We have been having some problems with a BGA device where we see
> ball fatigue (solder ball cracks) after temp cycling. We think it
> may be related to severe undercut of the solder mask.
>
> Does anyone have information on different solder mask foot
> profiles? How difficult is it to get a straight sidewall on
> solder masks?
>
> Are there any that are much better than others for this
> attribute? What would be the trade offs?
>
> You can contact me off line if you prefer.
>
> Steve Joy
> 503-696-2239
> [log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
David Gonnerman
Director of Publications
Plan now to attend:
Surface Mount International (San Jose, CA; 8/23-8/27)
Electronics Assembly Expo (Providence, RI; 10/24-10/29)
SURFACE MOUNT TECHNOLOGY ASSOCIATION
Enabling members to achieve success
in surface mount and companion technologies
through education, training and access to knowledge.
5200 Willson Road, Suite 215, Edina, MN 55424-1343
612-920-7682 F 612-926-1819
[log in to unmask] www.smta.org
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|