Hi Rob,
I am assuming that you are talking about attaching insulated, stranded
wires to a thru hole on a board.
1. Stranded wires are best pretinned.
2. They should be treated much like a solid wire or a component lead. i.e.
They should be visible on the secondary side, should not extend so far as
to be a threat for shorts, and should have a sufficient solder fillet on
top and bottom.
3. There should be sufficient insultion clearance.
4. You should still be cautious about solder wicking up under the
insulation into an area that needs to flex.
Hope this helps.
Charlie B.
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] Wires being used on PCB Assemblies
My name is Rob Carver at Harrington Signal Inc. in Moline Illinois.
Our Quality Assurance Supervisor recently quit and the inspectors have a
question that I as a ISO manager cannot answer, so I'll post a message.
The question is must wires that are soldered directly to PCB assemblies
be:
a. Pre-tinned??
b. Have both top and bottom side solder and the correct percentage
of fill.
The IPC book doesn't really address this point.
Rob Carver
Harrington Signal Inc.
2519 4th Avenue
Moline, Illinois 61265
1-800-577-5758
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|