Mime-Version: |
1.0 |
Sender: |
|
Subject: |
|
From: |
|
Date: |
Thu, 25 Jun 1998 12:08:07 +0300 |
Content-Type: |
text/plain; charset="us-ascii" |
Reply-To: |
|
Parts/Attachments: |
|
|
At 13:07 24/06/98 -0700, you wrote:
>Gabriela Bogdan wrote:
>>
>> Hi, TechNetters!
>> Could you please share with me your experience about pro and con's
>> regarding solder mask
>> between fine pitch-16mil- pads in relation to the finish of the PCB pads
>> ?
>> Not being greedy, I'll save the next question for after some answers.
>> Thank you,
>> Gaby
>>
Gaby ,
Untill now you got answers from assembly peoples and not from manufacturing
area .
Limitations on solder mask between fine pitches are coming mainly from image
transfer :
1 ) resolution of photoimagible solder mask : depends on solder mask itself
, exposure system and artwork . Generally ,( depends on type of soldermask
used ) , soldermask is lower than pads , so there is always gape between
soldermask and the artwork ( contrary to circuitry photoresist , that is in
contact with artwork ) .
2 ) registration problems : circuitry registration is according to drilled
holes , soldermask according to circuitry . Add to this type of artwork :
first generation or diazo and coresponding dimensional stability of the
artwork .
3 ) adhesion of " soldermask dam " to dielectic base depends also on width
of the " dam " . Neglecticing of this point will lead to " washing out " of
soldermask in developing stage ,during solder ( HASL ) application or even
during assembly .
These points should be known to each PCB manufacturer , otherwise he will
supply PCB without " dams " or with " dams " on SMT pads .
Regards
Edward
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|