Ed,
We use a powerful in-line claener on our assembled boards. We had stainless
steel wire mesh baskets made in different thicknesses to accomodate our
assembled boards.
Charlie B.
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Eltek Ltd. - Process Engineering" <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Charles Barker/US/I-O INC)
Subject: [TN] Washing of small PCB
Technetters,
After routing stage the PCBs are washed to remove dust , fingerprints etc .
Normally , this is done using washing machine fitted with hot water rinse ,
soft brushes , high pressure rinse , DI rinse and dryer . As long as the
PCB
is bigger than , say , 7" by 4" , we have no problems . Probles are with
really small boards such as 2" by 3" or even less .
What kind of washing machines are used for such small boards ?
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|