Hi Chris,
If your gold deposit is high in base metal content ( > .5%), eg cobalt or
nickel, then tarnishing will occur. Please confirm the alloy for excessive
brighteners and/or impurities. Additionally, field tarnishing may occur if
installed. Technic at 401-681-7100 for a cleaner.
Good Luck,
Lenny Kurup
EMX Enterprises Ltd
Markham, Ontario, Canada
On Wed, 10 Jun 1998, Chris Rucinski wrote:
> TechNetters,
>
> Is there chemistry available to remove oxidation
> from gold tips without compromising
> solderability?
>
> More specifically we have a costumer that has
> sent back some boards that have been stored
> for almost a year. The gold tips are tarnished.
> The customer has requested that we rework the
> boards, without out buffing the gold out. An
> analysis of the thickness gives 40 microinches
> of gold on 300 microinches of nickel.
>
> Many thanks,
>
> Chris Rucinski
> Process Eng.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|