Hi All,
- HEEEEELP!!!!!! I have an interesting dilemma.
We are trying to develop a circuit pattern to create a resistance of 9
milliohms. This circuit is also required to fuse between 5.0-6.0 amps.
The circuit will be formed on 2 oz. cu., exposed from soldermask and
will be solder coated to IPC standards. Operating temperature is 65C
degrees. I have some generic information concerning copper resistivity
from IPC-D-317A. This spec also refers to IPC-MF-150 for further
detail. I do not have this spec. Any info would be greatly
appreciated.
Thanks,
Rick
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|