Colin,
I believe that Gould used to manufacature Ni foil with a treatment for
bonding. the Ni foil is still in the MF 150 spec, so someone must still
offer it. You could try contacting all the foil vendors.
Dave McGowan
-----Original Message-----
From: Colin <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, May 28, 1998 6:48 AM
Subject: [TN] Nickel foil
>Fellow Technetters,
>
>I have had a request from one of my UK customers, where it would be
>possible to source FULLY ANNEALED nickel foil.
>
>He is looking for 18uM thick foil, treated preferably on both sides, but
>one will suffice, in panel sizes around 18" x 12" or 24" x 18".
>
>Any leads as to where I might get this material, either in Europe or
>Stateside?
>
>Either reply via TechNet, or off-line.
>
>Thanks in advance.
>
>Colin McVean
>Polyclad Technical Services UK
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|