Hi Guys,
I have a problem with dimensional stability of photo tools. The photo
tools shrink after processing. I've tried increasing the drying
temperature (50-55C) just so it will not shrink but it still does. This is
really giving me a headache. Any suggestions?
Marco Biagtan
NEC-CPI Process Engineer
------End Included Message---------------
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
The problem with silver halide film is it's dimensional stability to humidity
changes. Silver film specs quote dimensional stability to be .012% per deg RH
change over 24 inches, whereas the thermal coefficient is .0009% per deg F for
7 mil film.
The solution is to switch to a dry process system using dry plot film which has a thermal coefficient of .00085% per deg F for 4 mil film and a humidity
coefficient of .0009% per deg RH.
Dick Desrosiers
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|