Hi technetters,
I have a problem at wave solder with spikes on a BNC connector.
The spikes are on the ground pins which are 1.6mm diameter protruding 1.4
mm with a flat surface. The land diameter is only.4mm which may be causing
a problem..
we use turbulent to heat the part to some effect but does not clear the
problem entirely.
any clues
Rgds
Donal o Brien
################################################################