Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Wed, 13 May 1998 10:01:38 -0700 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
What do you want to know??
Raw Board Reliability (solderability)
Contact Resistance Reliability?
Solder Joint Reliability
With regards to Solder Joint Reliability, the solder interface of the
nickel to solder forms tin intermetallics which will not be as strong
as solder to solder. These joints will still be acceptable for most
smt components but immersion gold and BGA's should be avoided.
Regards:
Steve O'Hara HP
______________________________ Reply Separator _________________________________
Subject: [TN] Reliability of Immersion Gold PCB
Author: Non-HP-Fulton.Feng.ffeng ([log in to unmask]) at
HP-Vancouver,mimegw10
Date: 5/12/98 5:39 PM
Hi
Has anyboy done any reliability study on Gold Immersion PCB finish?
Thanks
Fulton Feng
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional inform
ation.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-97
00 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|