All,
To clarify my earlier posting....
It isn't that our oven has ever exhibited heat loading
problems. In fact, I plan on some heat loading experiments
to prove this. I just have an external customer who likes
to help. The problem is they are 100% convinced of the
following:
1) We absolutely have to have nitrogen on our reflow oven.
2) We have to place buffer boards before and after each
production assembly or else our heaters won't handle the
load properly.
I do appreciate all the responses so far, although more
opinions are welcomed and encouraged.
Thank you all for your help.
Steve McBride
[log in to unmask]
(405) 624-5281
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################