Chris,
Great Western Chemical has a process called MRA-D that works very well at
droping out copper in solution. The copper comes out as copper metal. The
benefits are that generates very little sludge and is a very simple
treatment.
Please give me a call at (612) 688-8533
Boyd Anderson
Great Western Chemical Co.
Eagan, MN
-----Original Message-----
From: [log in to unmask] <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, May 07, 1998 11:26 AM
Subject: [TN] Crashing copper
>I have a question about copper. I have a solution of copper nitrate and I
>want to crash all of the copper out of this solution. How would I go about
>doing this?
>
>Chris Coon
>Borden Chemical
>Kent, WA
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|