TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Nick Nicolaides <[log in to unmask]>
Date:
Thu, 28 May 1998 18:07:34 -0400
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Nick Nicolaides <[log in to unmask]>
Parts/Attachments:
text/plain (18 lines)
Exposed copper on solder resist is considered a non conformance per IPC600.
I can understand exposed copper with OSP since it does burn off during
Reflow and Wave soldering. In some cases copper is not tin lead. In several
operations, we seem to have the solder mask peel off slightly exposing
copper. Should this be acceptable similar to OSP.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2