TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"<Jason M. Smith>" <[log in to unmask]>
Date:
Wed, 27 May 1998 14:30:36 -0400
Content-Type:
text/plain; charset=us-ascii
X-To:
Greg Kilinski <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (58 lines)
The problems I see is that you have to overheat the solder to get a good
flow.  The actual temps, you have to experience from what I know.

Jason





Please respond to "TechNet E-Mail Forum."
      <[log in to unmask]>; Please respond to Greg
      Kilinski <[log in to unmask]>

To:   [log in to unmask]
cc:    (bcc: Jason Smith)
bcc:  Jason Smith
Subject:  [TN] Wave Soldering with Sn10




          Does anyone have experience wave soldering with Sn10/Pb90 solder?
My
          concern is the plastic (non-eutectic) melting range of 268-302 C
          (514-576 F), which may cause sluggish solder flow. Are there any
other
          areas of concern?

          Thanks in advance.

          [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2